ALUMINIUM FASTENERS - MAIN CHEMICAL & PHYSICAL CHARACTERISTICS
MATERIAL – 7075 GRADE HIGH TENSILE ALUMINIUM ALLOY WITH T73 HEAT TREATMENT
HEADS COLD FORMED WITH ROLLED THREADS
HIGH RESISTANCE TO CORROSION AND THE ELEMENTS
COLOUR ANODISED OR POTASSIUM BICHROMATE FINISH TO BETWEEN 8 & 12 MICRONS
60% LIGHTER THAN STEEL
TENSILE STRENGTH – 490-560 MPa
MECHANICAL PROPERTIES – SUPERIOR TO THOSE OF MILD STEEL
CAN BE USED IN ALL NON - CRITICAL SAFETY AREAS.
|
MAXIMUM TIGHTENING TORQUE |
|
M5 |
2.21 ft-lbs/3.00 Nm |
|
M6 |
3.69 ft-lbs/5.00 Nm |
|
M8 |
7.39 ft-lbs/10.00 Nm |
|
M10 |
14.38 ft-lbs/20.00 Nm |
*THE INFORMATION GIVEN IS FOR GUIDANCE ONLY AND SHOULD NOT BE USED TO ESTABLISH SPECIFICATION LIMITS.
|
SOCKET HEAD CAPSCREW |
| |
A |
B |
C |
|
|
M5 |
8.5 |
4.5 |
4 |
|
|
M6 |
10 |
7 |
5 |
|
|
M8 |
13 |
9 |
6 |
|
|
M10 |
16 |
12.5 |
8 |
|
|
HEXAGON |
| |
A |
B |
|
|
|
M5 |
8 |
3.5 |
|
|
|
M6 |
10 |
4 |
|
|
|
M8 |
13 |
5.3 |
|
|
|
M10 |
17 |
6.4 |
|
|
|
FULLNUT |
| |
A |
B |
|
|
|
M5 |
8 |
4 |
|
|
|
M6 |
10 |
5 |
|
|
|
M8 |
13 |
6.5 |
|
|
|
M10 |
17 |
8 |
|
|
|
NYLOC NUT |
| |
A |
B |
|
|
|
M5 |
8 |
5 |
|
|
|
M6 |
10 |
6 |
|
|
|
M8 |
13 |
8 |
|
|
|
M10 |
17 |
10 |
|
|
|
WASHER |
| |
A |
B |
|
|
|
M4 |
10 |
0.8 |
|
|
|
M5 |
12 |
1 |
|
|
|
M5 |
16 |
1 |
|
|
|
M6 |
14 |
1.2 |
|
|
|
M6 |
18 |
1.6 |
|
|
|
M8 |
18 |
1.6 |
|
|
|
M10 |
22 |
2 |
|
|
|
COUNTERSUNK WASHER |
| |
A |
B |
C |
D |
|
M5 |
22 |
3 |
|
|
|
M6 |
22 |
3 |
|
|
|
M8 |
25 |
5 |
|
|
|
SOCKET COUNTERSUNK |
| |
A |
B |
C |
|
|
M5 |
10 |
2.8 |
3 |
|
|
M6 |
12 |
3.3 |
4 |
|
|
M8 |
16 |
4.4 |
5 |
|
|
SOCKET BUTTON HEAD |
| |
A |
B |
C |
|
|
M5 |
12 |
3.7 |
3 |
|
|
M6 |
16 |
4.5 |
4 |
|
|